Page 1 of 1

body work

Posted: Sun Jun 04, 2006 7:09 pm
by matthewK
hey guys,

im just doing some body work to the roof of the nissan , now im using stuff called metal Tech has stainless steel in the mix too make it stronger then normal bogg,
i put this stuff on a week ago now and its still not dryed out and harden , i put the old bar heater out on it to try dry it up but nothing in fact it make the mix soft and tacky , its driving me nuts ,
now iv bogged before with normal bogg and it taken half the time of this metal tech ,

just wanna get the nissan back on the road so i can get the landcruiser in the garage to look at wheel bearings :)

any help will be good

Posted: Sun Jun 04, 2006 7:26 pm
by munga
scrape it out mate. you didnt mix it incorrectly did you? if not, take it back and get a refund. maybe the catalyst is out of date.

Posted: Sun Jun 04, 2006 8:22 pm
by matthewK
not at all i did put a tad more hardner then i should of thats about it ,
i got this stuff from super crap , last metal fill i used was from repco simlar stuff stainless in it id says it more out of date i'll pic up some new stuff tomorrow from repco i think